Pungent and unpleasant odors may be released during printing. Make sure your printer is enclosed and placed in a well-ventilated area.
When layer strength is required, it is recommended to increase the flushing volume to above 800 mm. If the flushing is not thorough, it may reduce the layer adhesion of the model at surfaces that are on the same horizontal plane as the support surface.
By increasing the “initial layer speed”, a more peelable support can be obtained. However, this will increase the risk of warping.
Dry out before use for higher print quality. Drying conditions: 80 for 4 hrs in the blast drying oven; 85 – 95 for 6 hrs in the X1 Series Heatbed. Please refer to Filament drying instructions on WIKI.
For more support-related settings, please refer to Support on WIKI.