Description

GF30 PA6 Pellets [30% Glass Fiber Nylon 6]

Processing Recommendations:

  • Pre-dry before extrusion at 90Àš °C for 4-6 hours. Àš A toaster oven works fine for this. Àš Do your family a favor and do not dry the resin in your kitchen oven! Àš (Wet material will extrude with bubbles present in the filament. Àš If this happens, dry the resin more before processing.)
  • Extrusion Temp:Àš 220-240Àš °C (depending upon how your heater bands, thermocouple, and PID are configured.)

Additional information

Filament Material

PA6-30GF

Pellet Kg Amount

25kg, 10kg